Here you can access material datasheets for our wide range of alloys and materials. Contact us if you need more information about our materials.
Standard:
A pure nickel alloy (Ni alloy) with a controlled carbon content of max. 0.02%.
View datasheet for:
A ferritic iron-chromium-aluminium alloy (FeCrAl alloy) for use at temperatures up to 1300°C (2370°F). Kanthal AF is characterized by excellent oxidation resistance and very good form stability.
Several product forms available:
A ferritic iron-chromium-aluminium alloy (FeCrAl alloy) for use at temperatures up to 1300°C (2370°F). Kanthal D is characterized by high resistivity and good oxidation resistance.
A copper-manganese-nickel alloy (CuMnNi alloy) for use at room temperature. Manganina 43 is characterized by very low thermal electromotive force (emf) compared to copper.
A ferritic iron-chromium-aluminium alloy (FeCrAl alloy) for use at temperatures up to 1400°C (2550°F). Kanthal A-1 is characterized by high resistivity and very good oxidation resistance.
A nickel-iron alloy (NiFe alloy) for use at temperatures up to 600°C (1110°F). The alloy is characterized by very low resistivity and high temperature coefficient of resistance.
An advanced powder-metallurgical, dispersion-strengthened, ferritic iron-chromium-aluminium alloy (FeCrAl alloy) with an addition of molybdenum. The alloy is suitable for furnace temperatures up to 1250°C (2282°F).
An advanced powder-metallurgical, dispersion-strengthened, ferritic iron-chromium-aluminium alloy (FeCrAl alloy) with exceptional form stability and oxidation resistance. It is suitable for furnace temperatures up to 1250°C (2282°F).
An austenitic nickel-chromium alloy (NiCr alloy) used for the positive leg of thermocouples type E or type K.
An austenitic nickel alloy (Ni alloy) used for the negative leg of thermocouples type K.